Higher productivity, higher deposition rates and improved wetting properties compared to solid wires with comparable analysis. Excellent weld metal quality and X-ray soundness.
Not required
- Cap layers for joining refractory Cr-Al-Si steels.
- Cladding corrosion resistant overlays.
- Cladding heat resistant overlays up to 1100ºC.
- Cladding components in a sulphurous environment.
- Cap layers for joining refractory Cr-Al-Si steels.
- Cladding corrosion resistant overlays.
- Cladding heat resistant overlays up to 1100ºC.
- Cladding components in a sulphurous environment.
Higher productivity, higher deposition rates and improved wetting properties compared to solid wires with comparable analysis. Excellent weld metal quality and X-ray soundness.
1.4710, 1.4712, 1.4713, 1.4722, 1.4724, 1.4729, 1.4740, 1.4742, 1.4745, 1.4762, 1.4773, 1.4776, 1.4820, 1.4821, 1.4822, 1.4823
G-X30CrSi6, G-X40CrSi23 TP433, X10CrSi6 502, X10CrAl24 TP443, X10CrAl7 502, X8Cr30, X10CrSi13, G-X40CrSi29, X10CrAl13 TP405-CA15, G-X12CrSi 26 5, G-X40CrSi13, X20CrNiSi 25 4 TP329, G-X40CrSi17, G-X40CrNi 25 4 TP329, X10CrAl18 430B-TP430, G-X40CrNiSi 27 4 TP329HC
AISI 327, ASTM A297HC






| Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Hardness |
|---|---|---|---|---|
| As Welded | >450 | >650 | >15 | 94 HB |